Raw melting material - aluminum scraps, cans, engine waste etc.
Output capacity - 5-30 tons/h, customized
Automation - Full automatic/ half automatic (based on output requirement and investment budget
Ingot type - ADC12 (7.5kg/ 10kg / customized)
1. After cleaning the oil and grease of waste aluminum, manually put it into the furnace with a forklift;
2. Ignition for melting furnace .Heat up to 680C, and input appropriate proportion of alloy elements. Heat up to 800C, melt and stir evenly, then fetch samples to the spectrometer for testing.
Every lot of production need to do testing .
3. Put A tool that attracts iron into the furnace by forklift, to suck away the iron in the aluminum water.
4. Put the slag agent into Alu liquid to remove the slag. After slag removed , put the slags into Aluminum ash separation machine , and let the aluminum water and ash separate. The proportion of slag agent and aluminum liquid is 1:500
5.Open the drain valve and the aluminum water flows automatically to the ingot production line After the ingot casting is completed, the ingot stacking robot will stack the ingots, which means the production is completed.
We supply high-purity Zinc Alloy for industrial applications, ensuring exceptional quality and performance. Our material features a Zinc (Zn) content of 99.999%, with extremely low levels of impurities, making it suitable for critical uses across multiple industries.
Applications:
This high-purity zinc alloy is ideal for:
Electronics and semiconductors
Galvanization processes
Specialty coatings
Advanced alloy manufacturing
Research and development
With our stringent quality controls and reliable delivery network, we ensure that your specific requirements are met with excellence. Contact us for further information or to request a quote.
Incoloy 825 is a nickel iron chromium alloy, which is widely used in petroleum, natural gas and chemical processing industries. It has good corrosion resistance and can operate at higher temperatures than most stainless steels. Incoloy 825 is a completely austenitic nickel iron chromium alloy, stabilized by titanium and added with copper and molybdenum. Incoloy 825 is a general engineering alloy, which is resistant to acid and alkali metal corrosion in oxidation and reduction environments.
The Incoloy825 has the following functions:
Good resistance to stress corrosion cracking.
Good resistance to pitting and crevice corrosion
Good oxidation resistance and non oxidative thermal acidity.
It has good mechanical properties at room temperature and high temperature up to 550
Certification of pressure vessels with manufacturing temperatures up to 450 C
Incoloy 825 metallographic structure:
Incoloy 825 alloy has a stable face centered cubic structure. Chemical composition and appropriate heat treatment ensure that the corrosion resistance will not be weakened by sensitization.
Incoloy825 Corrosion resistance:
Incoloy825 is a general engineering alloy, which is resistant to acid and alkali metal corrosion in oxidation and reduction environments.
Incoloy825 is widely used in various industrial fields where the working temperature is no more than 550.
Typical applications include:
Heating pipes, containers, baskets and chains for sulfuric acid pickling plants.
Seawater cooling heat exchanger, marine product pipeline system, acid gas environment pipeline.
Heat exchanger, evaporator, washing, immersion tube, etc. In phosphoric acid production.
Air heat exchanger in petroleum refining
Food Engineering
chemical process
Flame retardant alloy for high-pressure oxygen
Product name
INCOLOY Alloy 825
Grade
INCOLOY Alloy 825
Thickness range
0.3mm-3.0mm,
Width range
600mm-1500mm
Length
2000mm, 2438mm, 3048mm
Size
1000mm*2000mm, 1219mm*2438mm, 1219mm*3048mm, or as required
The third-generation Hastelloy alloy alloy20 is one of the more commonly used components in the C series. Due to its low nickel content, low cost, excellent mechanical and corrosion resistance, it is widely used in pump flow components where corrosion and wear coexist. The solubility of hardness in the ferrite phase reaches its maximum at 850, and as the temperature increases, the solubility increases rapidly and is much smaller than that of the austenite phase. The Cu content in c-276 has exceeded the high solubility in the ferrite phase.
The Hastelloy alloy alloy20, formed by a large amount of Ni element composition, is used in industries such as chemical engineering, pharmaceuticals, seawater, fertilizers, and other industries for projects with high corrosion resistance requirements due to its unique characteristics that lie between ferrite and austenite structures, and its resistance to intergranular corrosion. In recent years, the nuclear power industry has developed a corrosion-resistant ability in the operation of power station equipment, which cannot be replaced by other materials. Containing a large amount of Cr component, with high oxidation resistance.
The molybdenum element in stainless steel materials is only about 2%, which is far less than the molybdenum content of Hastelloy alloy alloy20. Therefore, high concentration acidity requires the use of materials well. Mainly used, it has the following corrosion resistance properties in oxidation and reduction, and excellent corrosion resistance to most corrosive media. In this oxidizing environment, such as in sulfuric acid manufacturing and solutions containing a large amount of oxidizing ions, it has excellent resistance to pitting corrosion, crevice corrosion, and stress corrosion.
Product name
ALLOY 20 STAINLESS STEEL
Thickness range
0.3mm-3.0mm,
Width range
600mm-1500mm
Length
2000mm, 2438mm, 3048mm
Size
1000mm*2000mm, 1219mm*2438mm, 1219mm*3048mm, or as required
Interior/exterior/architectural/bathroom decoration, elevator decoration, hotel decoration, kitchen equipment, ceiling, cabinet, kitchen sink, advertising nameplate
Warehouse Storage
Shandong Jintuo Metal Materials Co., Ltd is located in Liaocheng City, the capital of steel tubes. It is a large enterprise specializing in the sales of carbon steel, stainless steel, galvanized color coated products, and copper and aluminum.Our company adopts a flexible business approach and management mechanism to provide good services to customers, while also considering the interests of the owner and the project, in order to ensure the quality of the project.
Use of INCOLOY Alloy 825: 1. The heater is generally used in the oil refining unit; 2. Chemical plant equipment pipeline; 3. Fast cooling cylinder for solid solution used in textile industry; 4. Seamless steel pipe for heat exchanger and condenser. 5. High pressure seamless steel pipe for food (gb-2000) is a high-quality carbon structural steel and alloy steel seamless steel pipe suitable for chemical equipment and pipes with working temperature of - 40~400 �° C and working pressure of 10~30ma. 6. Seamless steel pipes for geological drilling and oil drilling control. 7. Cracking pipe for petrochemical industry is used to transport high-temperature and high-pressure fluid on fertilizer equipment.
INCOLOY Alloy 825
Standard
Food Grade Sanitary Tube: JIS G3447, KS D 3585, ASTM A270, EN 10357(DIN 11850), AS 1528.1, ISO 2037(NF A49-249)
Industrial pipe: ASTM A312, EN 10217-7, GB / T 12771-2008, HG 20537.3
Drinking water tube: GB / T 19228
Mechanical tube: ASTM A554, EN 10296-2
Size
Outer Diameter Range: 9.5~2000mm
Thickness Range: 0.5~20mm (Size can be customized.)
Length: Up to 11.8 meters per piece.
Shape Section
Round, square, rectangular
Usage
Sanitary tubing: for food processing industry, beverage industry, sugar mill and so on;
Heat exchanger tube: condenser, boiler, super heater, evaporator and so on;
Industiral pipe: for petroleum delivery, gas delivery, petrochemical industry, wastewater treatment, drainage system, and so on;
Mechanical tube: handrail, railings, balustrade, hence and so on.
Features:
1.Our stainless steel tubes pipes are treated by bright annealing, inside weld bead removing, precise polishing. The roughness of tubes could be under 0.3�¼m.
2.We have the non destructive testing ( NDT ), eg. online eddy current inspection and hydraulic or airtightness testing.
3. Thick welding, good appearance.The mechanical properties of tube could be tested.
4. And Our tubes are certificated by AD 2000-W0, PED 2014/68/EU, ISO 9001 : 2015.
5. Full material traceability is guaranteed during the manufacturing process.
6. Polished tube is supplied in individual plastic sleeves with capped ends ensuring optimum cleanliness.
7. Internal Bore: Tubes have a smooth, clean and crevice free bore.
We also have interest in selling Bulk Ferro Alloys and especially Low/Medium Carbon Silico Manganese and we are already exporting these product/s. We have tied up with a manufacturer bin , Bhutan to sell their products.
We are engaged in making Lead available in several forms including
LME registered and non registered 99.97% and 99.99% as well as
secondary ingots, foil, granules, powder, rod, shot, sheet, and wire.
Lead is a bluish-white lustrous metal. It is very soft, highly malleable, ductile, and a
relatively poor conductor of electricity. It is very resistant to corrosion but tarnishes
upon exposure to air. Alloys include pewter and solder.